Sealed Insulating Glass Thomsonite Molecular Sieve Adsorbent Selling
Product Introduction of Molecular Sieve Adsorbent:
Our company production of the molecular sieve as a special insulating glass desiccant, can continuous hollow glass interval layer adsorption of water depth and the residual organic matter, effective prevent dewing frosted glass, thoroughly solve the insulating glass distortion caused by the expansion and contraction and broken problem, ensure the service life of hollow glass shortest more than 20 years.
Technical Parameters of Molecular Sieve Adsorbent:
Specification | |||||
Unit | Value | ||||
Bead Size | mm | 0.5-1.0 | 1.0-1.5 | 1.5-2.0 | |
Bulk Density | g/ml ≥ | 0.72-0.82 | 0.70-0.80 | 0.68-0.78 | |
Equilibrium Water Capacity @ 25℃ | wt% ≥ | 19.0-21.5 | 19.0-21.5 | 19.0-21.5 | |
Equilibrium Nitrogen Capacity | mg/g ≤ | 2.0 | 2.0 | 2.0 | |
Heat of Adsorption | BTU/lb of H2O | 1800 | 1800 | 1800 | |
Crush Strength | Point Contact | N ≥ | - | 10-20 | 30-50 |
Variable Coefficient | - | 0.3 | 0.3 | 0.3 | |
Dust(Turbidity Meter) | ppm ≤ | 30 | 30 | 30 | |
Delt (10g/10ml H2O) | ℃ ≥ | 40 | 40 | 40 | |
Dew Point | ℃ ≤ | -73 | -73 | -73 | |
Loss of Ignition(950℃) | wt% ≤ | 2 | 2 | 2 | |
Size Qualification | % ≥ | 96 | 96 | 96 | |
Package Moisture | wt% ≤ | 1.5 | 1.5 | 1.5 | |
The interval value of the indexes above are based on the grades of Insulated Glass Drier |
Photo of Molecular Sieve Adsorbent:
FAQ of Molecular Sieve Adsorbent:
1. Q: Could we send a free sample for reference?
A: Yes, of course. Don't hesitate. Go ahead & ask for a sample.
2. Q: What about the price and MOQ?
A: We promise the price is better competitive with good quality. we accept both large and small quantity orders.
3. Q: What is the lead time?
A: Within 20 days after the receipt of payment or L/C.
4. Q: Payment term?
A: 30% T/T in advance, 70% T/T balance before shipment.
5. Q: How to solve the quality problems after sales?
A: Take photos of the problems and send us. After confirmation, we will provide solutions within 3 days.
For more information please contact us. It's our pleasure to solve the question for you.
The attention of Molecular Sieve Adsorbent:
1. The product cannot be exposed in the open air and should be stored in dry condition with an air-proof package.
2. The product should be regenerated after a certain period of adsorption. The appropriate regenerated temperature would be better below 350°C.